You return home after a long journey. Imagine being greeted by a beautiful stainless steel sculpture surrounded by landscaped gardens on your return. One ASSDA Member has used stainless steel to symbolise everything we love about our communities: Security, comfort and home.

It’s easy to think of stainless steel in relation to tubes, panels and rolls in the construction industry, but Brisbane-based ASSDA member, Concept Stainless Design, has taken the product and crafted it into stunningly beautiful sculptures for developers Villa World at their new subdivision on the northern Gold Coast.

Located 70km south of Brisbane, Arundel Springs will provide 386 dwellings in a family-friendly environment adjacent to the Coombabah Lakelands Conservation Area and close to Griffith University and light rail services.

Villa World provided the concept design to reflect the organic growth of nature and symbolise the new families and children who will grow in the new suburb. 

The team at Concept Stainless Design adapted the design to match the size of available grade 316 stainless steel sheets. A small curve of 5mm radius was provided at the tip of the fronds to avoid sharp edges. Another small curve of 9mm was used at the gully between fronds to achieve a flawless polished finish.

The sculptures have been designed to withstand winds of up to 160km per hour, an important feature given Arundel Spring’s proximity to the ocean. An internal frame was built to secure the fronds in position, as well as a horizontal base beam hidden within the sculpture and two legs extending down from the base beam into a large buried concrete block. The structural design certification was completed by Concept Stainless Design’s in-house engineer.

The face of each sculpture was manufactured from grade 316 stainless steel sheet supplied by ASSDA Sponsor Dalsteel Metals.

The sculpture faces are joined along the centre line with an invisible polished butt weld, executed by Concept Stainless Design’s highly skilled tradesman at their Brisbane workshop. The faces were bonded to marine ply and “U” stiffeners were formed from grade 316 stainless steel strips then glued and screwed in. The second face was then placed over the stiffeners, glued and screwed to the ply-bonded face.

The entire project took eight weeks to construct and transported to their new home at Arundel Springs. The sculptures were secured in place by concrete blocks and steel bolts provided by Villa World’s civil contractor in under two hours.

Stainless steel was chosen for the sculptures because of its beautiful, smooth and highly polished finish, and for its low-maintenance properties. Surrounded by clear skies, new vegetation and lush grass, the sculptures welcome residents and visitors alike.

This article is featured in Australian Stainless Magazine Issue 60 (Summer 2017/18).