20 November 2017
The new facility in Merrifield Estate on Melbourne's outer northern fringe will allow Dulux to step into the next generation of paint manufacturing technology and innovation. Dulux's aim was to design and construct a state-of-the-art facility, so using quality products was essential to achieve this. Stainless steel in 300 series grades was an integral part of the project design, including storage vessels and over 10,000m of food grade, quality tube complying with AS1528.