Alloy C-276: A Super Alloy for Processing Plants

Alloy C-276: A Super Alloy for Processing Plants

OMG Cawse Pty Ltd is the owner and operator of a nickel and cobalt mining operation and processing plant that is located 55 kilometres north east of Kalgoorlie.

Extracting nickel involves acid leaching using sulfuric acid in a high temperature and pressure autoclave to dissolve the nickel and cobalt from the oxide ore.

The wastes from this process are very acidic and require a highly corrosion resistant material for the lining of the sump tank.

When various concrete coatings for the sump tank were trialed and failed, OMG Cawse opted to install Alloy C-276 to engineer out the continuous maintenance of the concrete coatings.

Alloy C-276 is a super nickel alloy (not a stainless steel), a material that remains resistant in the most corrosive environments such as in chemical processing, waste treatment, pollution control and pulp and paper production.

ASSDA member, Specialised Engineering Services (WA) fabricated a 3mm thick liner for a sump tank from Alloy C-276 plate supplied by ASSDA Major Sponsor, Atlas Steels.

Measuring 9m long x 2.5m wide x 1m to 1.3m deep, the tank is filled with water and receives up to 98% sulphuric acid.

Alloy C-276 is also one of the few materials that can withstand the corrosive effects of chlorine dioxide, wet chlorine gas and hypochlorite.

This article featured in Australian Stainless Issue 34 - Summer 2005.

ASSDA - Supporting You

ASSDA’s activities focus on networking, promotion, education, accreditation, standards development and problem-solving. View the Association's history of achievements and milestones in supporting the Australian stainless steel industry here.

160+

Member Organisations

100+

Publications

8,775+

Stainless Steel Specialist
Course enrolments

Check out our services

 

Stainless Steel Specialist Course

An online educational tool designed to improve your knowledge of stainless steel, its properties, performance and uses. Consisting of 17 challenging and rewarding modules, the course delivers a standard level of knowledge and qualification across the industry.

Learn more
 

ASSDA webinars

ASSDA's webinar program was introduced in late 2014, providing educational presentations on various stainless steel topics for Members, the specifying community and the stainless steel industry as a whole.

Learn more
 

Technical inquiries

ASSDA's Technical Support Service represents a significant asset to the local stainless steel industry, providing excellent and timely advice for the successful use of the product.

Learn more
 

ASSDA resources

ASSDA delivers a strong publications and training program with a range of titles available to participants in the stainless steel industry.

Learn more

Stainless Steel Industry Directory

As the go-to resource for the stainless steel industry in Australia, this directory is designed to showcase the capabilities of ASSDA Members and Accredited Fabricators while also serving as a platform to connect businesses with potential work opportunities.
Whether you’re a professional within the industry or a client seeking a specific stainless steel service, the Stainless Steel Industry Directory is here to facilitate connections and collaborations. Browse ASSDA’s Directory now to discover the businesses and services that can meet your stainless steel needs effectively and efficiently.

ASSDA Young Professionals Network

Empowering the next generation of stainless steel professionals and leaders.