Australian Technology Advances Industry

Australian Technology Advances Industry

A new technique for manufacturing high pressure cavity plate for heat exchange applications developed by the Australian stainless steel industry increases the options available to the food processing and manufacturing sectors. 

'Laser welded cavity plate' has been developed by ASSDA member J Furphy & Sons, a Shepparton fabricator of stainless steel tanks and processing equipment, as an alternative to resistance or plug welded dimple plate used for the heating or cooling jackets on stainless steel tanks, vessels and silos.

A wide range of industries stands to benefit from the new cavity plate, from dairy, brewing, food, wine, pulp and paper, chemical, pharmaceutical, refrigeration to textiles and manufacturing.

It is designed to be used in jacketed tanks, pressure vessels, shells and heads, troughing, chutes and hoppers, immersion plates, bank assemblies, baffles, ice-making plates, water chillers and food cookers.

The method of manufacture allows design flexibility enabling it to be tailored to specific performance requirements. It can be designed to suit both the flow characteristics of the refrigerant or heating medium and the required performance objective for the equipment by programming the cavity pattern and dimensions into a CNC controlled laser welding system.

The process involves laser welding two sheets of stainless steel in their flat form and inflating to form the cavity through which the cooling or heating medium is transferred.

The laser welds are exceptionally strong and have been burst tested in excess of 13 000 kPa, with most common demand being for operating pressures between 300 and 3 000kPa.

The product is available single embossed for uses where a flat inner wall is required or double embossed for immersion where both sides of the plate are utilised to heat or chill.

It is in use in chocolate crucibles in the confectionery industry as well as in Peerless Holdings’ edible oils processing tanks. Orbis Engineering has used the cavity plate in a cooling tunnel conveyor bed and Barry Brown & Sons has utlised it in on-farm milk silos. It has also been used in various major winery projects, including Peace Wines and Jindalee Estate, for fermentation and storage vessels.

Another ASSDA member, A&G Engineering of Griffith, has specialised in cavity plate for use as a cooling plate in wine vessels for a number of
years. This product also incorporates technology unique to Australia.

This article featured in Australian Stainless magazine - Issue 22, September 2002.

ASSDA - Supporting You

ASSDA’s activities focus on networking, promotion, education, accreditation, standards development and problem-solving. View the Association's history of achievements and milestones in supporting the Australian stainless steel industry here.

160+

Member Organisations

100+

Publications

8,775+

Stainless Steel Specialist
Course enrolments

Check out our services

 

Stainless Steel Specialist Course

An online educational tool designed to improve your knowledge of stainless steel, its properties, performance and uses. Consisting of 17 challenging and rewarding modules, the course delivers a standard level of knowledge and qualification across the industry.

Learn more
 

ASSDA webinars

ASSDA's webinar program was introduced in late 2014, providing educational presentations on various stainless steel topics for Members, the specifying community and the stainless steel industry as a whole.

Learn more
 

Technical inquiries

ASSDA's Technical Support Service represents a significant asset to the local stainless steel industry, providing excellent and timely advice for the successful use of the product.

Learn more
 

ASSDA resources

ASSDA delivers a strong publications and training program with a range of titles available to participants in the stainless steel industry.

Learn more

Stainless Steel Industry Directory

As the go-to resource for the stainless steel industry in Australia, this directory is designed to showcase the capabilities of ASSDA Members and Accredited Fabricators while also serving as a platform to connect businesses with potential work opportunities.
Whether you’re a professional within the industry or a client seeking a specific stainless steel service, the Stainless Steel Industry Directory is here to facilitate connections and collaborations. Browse ASSDA’s Directory now to discover the businesses and services that can meet your stainless steel needs effectively and efficiently.

ASSDA Young Professionals Network

Empowering the next generation of stainless steel professionals and leaders.