2205 Golden Choice for Mine Upgrade

2205 Golden Choice for Mine Upgrade

Two 2205 duplex stainless steel elution columns over 12 metres long have been installed in a replacement project at Kalgoorlie Consolidated Gold Mines in Western Australia. 

Elution columns are used in the mettalurgical process of extracting gold from carbon.

Carbon impregnated with gold is hot washed with caustic cyanide in the elution columns to dissolve the gold out of the carbon. The gold solution is pumped away while the barren carbon remains in the columns and then is removed for reuse.

The columns hold temperatures of 140°C and operate under pressures of 550 kilopascals (KPa).

he previous columns, constructed from grade 304 stainless steel, were beginning to fail due to pitting corrosion caused by chlorides carried over in the process water, combined with erosion corrosion on the internal surface. The tanks were in service for a total of five years.

Stainless steel supplier, ASSDA member Sandvik Australia, worked with a consultant to find a more suitable grade of stainless steel for the job.

2205 was chosen for its ability to provide a higher resistance to chloride attack. The grade also has improved hardness over grade 304, thereby offering better resistance to the erosion effect of the activated carbon.

Kalgoorlie Consolidated Gold Mines Mechanical Engineer Adrian Rowell, said the grade change was made to try to ensure the columns lasted the life of the mine.

"The plant is planned to operate for another 15 to 20 years," Mr Rowell said . "By shifting to 2205 we anticipate that the columns will last that long."

Fabricated by ASSDA member Specialised Engineering Services (WA) Pty Ltd, the columns were constructed from 2205 duplex stainless steel
8 millimetre plate, which offered a significant weight saving over the original 10 millimetre grade 304 vessel. The columns were fabricated to AS 1210 class 28 Pressure Vessels with a maximum design temperature of 150°C.

Each elution column is 12.4 metres long, 1.7 metres in diameter and positioned vertically.

This article featured in Australian Stainless magazine - Issue 18, May 2001.

ASSDA - Supporting You

ASSDA’s activities focus on networking, promotion, education, accreditation, standards development and problem-solving. View the Association's history of achievements and milestones in supporting the Australian stainless steel industry here.

160+

Member Organisations

100+

Publications

8,775+

Stainless Steel Specialist
Course enrolments

Check out our services

 

Stainless Steel Specialist Course

An online educational tool designed to improve your knowledge of stainless steel, its properties, performance and uses. Consisting of 17 challenging and rewarding modules, the course delivers a standard level of knowledge and qualification across the industry.

Learn more
 

ASSDA webinars

ASSDA's webinar program was introduced in late 2014, providing educational presentations on various stainless steel topics for Members, the specifying community and the stainless steel industry as a whole.

Learn more
 

Technical inquiries

ASSDA's Technical Support Service represents a significant asset to the local stainless steel industry, providing excellent and timely advice for the successful use of the product.

Learn more
 

ASSDA resources

ASSDA delivers a strong publications and training program with a range of titles available to participants in the stainless steel industry.

Learn more

Stainless Steel Industry Directory

As the go-to resource for the stainless steel industry in Australia, this directory is designed to showcase the capabilities of ASSDA Members and Accredited Fabricators while also serving as a platform to connect businesses with potential work opportunities.
Whether you’re a professional within the industry or a client seeking a specific stainless steel service, the Stainless Steel Industry Directory is here to facilitate connections and collaborations. Browse ASSDA’s Directory now to discover the businesses and services that can meet your stainless steel needs effectively and efficiently.

ASSDA Young Professionals Network

Empowering the next generation of stainless steel professionals and leaders.