Stainless Export Defies Elements

Stainless Export Defies Elements

Sixty tonnes of stainless steel has been exported to Hong Kong as part of an innovative Australian-designed and manufactured kit form, large span skylight project worth three quarters of a million dollars. 

The 42 gable trussed skylights and sub-frames in varying sizes up to four metres wide and eight metres long were installed in a $90 million dollar treatment plant commissioned by the Hong Kong Government.

Grade 316 stainless steel was used for the skylight's precision pre-cut sub-frame members, welded maintenance ladders, lntalok mechanism assemblies, special profiles, on sight assembly jigs, pivots and fixings.

The project specified that the skylights be easily removed from the roof to allow crane access to equipment in the building. However, the skylights also had to be strong enough to withstand Hong Kong's coastal gale force winds. Sky Roof International (Victoria) undertook the project.

Sky Roof Director, lan Howe, said the specifier's requirements and environmental concerns were met by adapting stainless steel to the company's lntalok cyclonic glazing frame system.

"The government specified that they wanted something striking, low maintenance and durable," Mr Howe said.

"As the frames had to be robust for lifting and withstand the conditions inherent in a coastal region, the obvious choice was stainless steel."

The skylight was designed to use wind uplift force to operate the lntalok hold down mechanism.

When the aluminium skylight structure is forced skyward by wind suction on the glazing, the small surface area of the stainless steel sub-frame is unaffected. This creates a differential force between the skylight and the sub-frame which is transmitted to the lntalok mechanism via the stainless steel ladders. The stronger the wind uplift on the skylight, the tighter the stainless steel lntalok engages the building.

All the prefabricated stainless steel components for the skylights were produced in a zircon glass bead blasted finish by ASSDA member Hart to Hart Fabrications (Dandenong, Victoria).

The skylights were then shipped to Hong Kong in fully fabricated kit form for easy on site assembly.

Mr Howe said ASSDA's Australian Stainless Reference Manual was vital in providing stainless steel technical and supply information.

"I found the Reference Manual and other pieces of information very useful in learning more about stainless steel and also in helping me find a fabricator for the job - Hart to Hart Fabrications," he said.

Following the success of the Hong Kong project, Sky Roof International is working on a design for a skylight featuring stainless steel glazing frames.

This article featured in Australian Stainless magazine - Issue 17, January 2001.

ASSDA - Supporting You

ASSDA’s activities focus on networking, promotion, education, accreditation, standards development and problem-solving. View the Association's history of achievements and milestones in supporting the Australian stainless steel industry here.

160+

Member Organisations

100+

Publications

8,775+

Stainless Steel Specialist
Course enrolments

Check out our services

 

Stainless Steel Specialist Course

An online educational tool designed to improve your knowledge of stainless steel, its properties, performance and uses. Consisting of 17 challenging and rewarding modules, the course delivers a standard level of knowledge and qualification across the industry.

Learn more
 

ASSDA webinars

ASSDA's webinar program was introduced in late 2014, providing educational presentations on various stainless steel topics for Members, the specifying community and the stainless steel industry as a whole.

Learn more
 

Technical inquiries

ASSDA's Technical Support Service represents a significant asset to the local stainless steel industry, providing excellent and timely advice for the successful use of the product.

Learn more
 

ASSDA resources

ASSDA delivers a strong publications and training program with a range of titles available to participants in the stainless steel industry.

Learn more

Stainless Steel Industry Directory

As the go-to resource for the stainless steel industry in Australia, this directory is designed to showcase the capabilities of ASSDA Members and Accredited Fabricators while also serving as a platform to connect businesses with potential work opportunities.
Whether you’re a professional within the industry or a client seeking a specific stainless steel service, the Stainless Steel Industry Directory is here to facilitate connections and collaborations. Browse ASSDA’s Directory now to discover the businesses and services that can meet your stainless steel needs effectively and efficiently.

ASSDA Young Professionals Network

Empowering the next generation of stainless steel professionals and leaders.