Stainless steel makes an entrance

Stainless steel makes an entrance

A collaboration between ASSDA Members using 'gold' stainless steel has delivered the epitome of opulent luxury at The Star Sydney.

The Star Sydney's multi-million-dollar transformation has seen its Pyrmont Street entrance revolutionise the guest arrival experience, with a porte-cochère facing the glittering Darling Harbour and a refurbished Grand Foyer combining innovative architecture, contemporary art and technology.

Over 4000m2 of grade 316 stainless steel with a gold finish is featured throughout the Grand Foyer and porte-cochère, enriching the luxurious look and feel of the integrated resort. ASSDA Member Steel Color Australia supplied 1mm and 1.2mm thick stainless steel sheet in various lengths from 2400mm to 3500mm and widths of 1219mm to 1500mm as the sole distributor in Australia and New Zealand for embossed, coloured, mirror finished and textured stainless steel manufactured by Steel Color S.p.a in Italy.

The stainless steel's gold colour was achieved with a titanium film using a Physical Vapour Deposition (PVD) coating process. The environmentally-friendly method vapourises titanium in a vacuum chamber to form an extremely thin layer that bonds to the steel's surface. The process also improves the performance of the steel, increasing durability and resistance to heat, light, abrasion, scratches and corrosion.

In addition, the steel's surface features an anti-fingerprint (AFP) coating preventing oil and finger marks, contributing to a sleek aesthetic finish with minimal maintenance. The AFP coating provides the titanium coating with a timer colour finish, strengthening colour stability and extending the service life of the application.

Suitable for internal and external applications, coloured stainless steel can be used in many design forms and was specified for the bespoke luxurious features in The Star Sydney's Foyer and porte-cochère.

The Steel Color Australia supplied stainless steel sheeting was installed in the Grand Foyer and internal porte-cochère by ASSDA Member Karisma Joinery, across the door portals, elevator door jambs and ceiling panels, columns and wall panels. A V-Groove machine was used to form precise, sharp angles and folds, creating architectural profiles to achieve a seamless upmarket finish and meet the high-end specification.

The stainless steel clad elements for the external porte-cochère, including luxury retailer finishes for Gucci, was fabricated and installed by ASSDA Member Fabmetal Specialists. All profiles and clad elements were fabricated in their workshop in Melbourne, using an in-house V-Groove machine to achieve a crisp bend profile, prior to installation on-site by the Fabmetal team. A split batten system was used to clad the stainless steel elements across the retail facade fixtures, window mullions, headers and kickers. The Fabmetal team were also tasked to clad the revolving doors and overcame challenges with complex curved works, laminating gold stainless steel on to curved fabricated T-sections in power-coated aluminium to create a striking two-tone effect.

In a nod to architectural innovation, The Star Sydney will continue to welcome and awe its guests with its everlasting stainless steel gleam and elegance.

  

 

PHOTO CREDIT: MURRAY FREDERICKS PHOTOGRAPHY. 

This article is featured in Australian Stainless Magazine issue 68, 2020.

 

ASSDA - Supporting You

ASSDA’s activities focus on networking, promotion, education, accreditation, standards development and problem-solving. View the Association's history of achievements and milestones in supporting the Australian stainless steel industry here.

160+

Member Organisations

100+

Publications

8,775+

Stainless Steel Specialist
Course enrolments

Check out our services

 

Stainless Steel Specialist Course

An online educational tool designed to improve your knowledge of stainless steel, its properties, performance and uses. Consisting of 17 challenging and rewarding modules, the course delivers a standard level of knowledge and qualification across the industry.

Learn more
 

ASSDA webinars

ASSDA's webinar program was introduced in late 2014, providing educational presentations on various stainless steel topics for Members, the specifying community and the stainless steel industry as a whole.

Learn more
 

Technical inquiries

ASSDA's Technical Support Service represents a significant asset to the local stainless steel industry, providing excellent and timely advice for the successful use of the product.

Learn more
 

ASSDA resources

ASSDA delivers a strong publications and training program with a range of titles available to participants in the stainless steel industry.

Learn more

Stainless Steel Industry Directory

As the go-to resource for the stainless steel industry in Australia, this directory is designed to showcase the capabilities of ASSDA Members and Accredited Fabricators while also serving as a platform to connect businesses with potential work opportunities.
Whether you’re a professional within the industry or a client seeking a specific stainless steel service, the Stainless Steel Industry Directory is here to facilitate connections and collaborations. Browse ASSDA’s Directory now to discover the businesses and services that can meet your stainless steel needs effectively and efficiently.

ASSDA Young Professionals Network

Empowering the next generation of stainless steel professionals and leaders.