Life cycle costing in the City of Melbourne

Life cycle costing in the City of Melbourne
Street furniture defines a city's urban landscape, and stainless steel is becoming a material of choice for its long-term cost benefits in addition to its sleek designs, durability, and visual appeal.

In Australia, the City of Melbourne has led the way in sustainable materials selection, undertaking a life cycle costing comparison study over a 25-year term between carbon steel and stainless steel for use in its public street furniture.

The products studied and manufactured included 1200 general waste bins, 500 recycling bins, 800 seats, 400 benches and 80 drinking fountains. Two broad costing components were considered:

  1. The initial (procurement) cost of the different products in two materials.
  2. The. ongoing maintenance costs, including costs associated with the following:
    1. Items physically destroyed when in situ and in service.
    2. Repairable damage to items when in situ and in service, e.g. graffiti
    3. Any required repairs due to natural corrosion and degradation.
       

The total cost of products made from carbon steel was $21.1 million:

  • $4 million in procurement costs.
  • $4 million in early replacement (re-procurement) costs.
  • $600,000 in maintenance costs (i.e. graffiti removal and re-coating of surfaces) per year.
     

The total cost of products made from stainless steel was $14.8 million:

  • $6.2 million in procurement costs.
  • $400,000 in maintenance costs per year.

 

Choose stainless steel

Stainless steel street furniture products realised a financial saving of $6.2 million over a 25-year term or $250,000 per year when compared with carbon steel. The stainless steel products are expected to last much longer than 25 years, delivering further cost savings for the City of Melbourne.

While there may be a higher capital cost initially, the benefits of using stainless steel are unmatched in its material performance and reduction in ongoing maintenance and life-cycle costs.

 

This article was adapted and originally published by World Stainless. Photo credit: City of Melbourne.

This article was featured in Australian Stainless Magazine Issue 77 (2023).

Authors

Lissel Pilcher

ASSDA - Supporting You

ASSDA’s activities focus on networking, promotion, education, accreditation, standards development and problem-solving. View the Association's history of achievements and milestones in supporting the Australian stainless steel industry here.

160+

Member Organisations

100+

Publications

8,775+

Stainless Steel Specialist
Course enrolments

Check out our services

 

Stainless Steel Specialist Course

An online educational tool designed to improve your knowledge of stainless steel, its properties, performance and uses. Consisting of 17 challenging and rewarding modules, the course delivers a standard level of knowledge and qualification across the industry.

Learn more
 

ASSDA webinars

ASSDA's webinar program was introduced in late 2014, providing educational presentations on various stainless steel topics for Members, the specifying community and the stainless steel industry as a whole.

Learn more
 

Technical inquiries

ASSDA's Technical Support Service represents a significant asset to the local stainless steel industry, providing excellent and timely advice for the successful use of the product.

Learn more
 

ASSDA resources

ASSDA delivers a strong publications and training program with a range of titles available to participants in the stainless steel industry.

Learn more

Stainless Steel Industry Directory

As the go-to resource for the stainless steel industry in Australia, this directory is designed to showcase the capabilities of ASSDA Members and Accredited Fabricators while also serving as a platform to connect businesses with potential work opportunities.
Whether you’re a professional within the industry or a client seeking a specific stainless steel service, the Stainless Steel Industry Directory is here to facilitate connections and collaborations. Browse ASSDA’s Directory now to discover the businesses and services that can meet your stainless steel needs effectively and efficiently.

ASSDA Young Professionals Network

Empowering the next generation of stainless steel professionals and leaders.