Fitness Never Looked So Good

Fitness Never Looked So Good

Sydney’s Fifty Four Park Street is not your average gym. The exclusive venue recently underwent a luxury makeover requiring 250 square metres of stainless steel to fully portray the club’s intended style and class. ASSDA Accredited Fabricator Townsend Group worked with designer Blainey North to create a stunning and sustainable interior.

Mirror finished columns are a focal point of the indoor pool, featuring circular column cladding joined with chrome coloured silicon to maximise waterproofing. Two of the columns double as large features with water pumped up the centre of each, to spill out and over the top.

Townsend Group’s Mark Ryan says the columns are constantly drenched in warm, chlorinated pool water, so grade 316 stainless with a No.8 finish was the best choice for corrosion resistance in the humid, damp environment.

Skirting, handrails, patch fittings, stair soffits, a dividing-wall feature and balustrades were mostly vee-cut prior to rolling or bending to achieve tight radii bends. All polishing was done by hand to a mirror finish to produce a highly reflective surface as specified by the designer.

“Blainey North specialises in upmarket fit-outs and is meticulous about workmanship and quality,” said Mr Ryan, who added that clean, reflective surfaces were a high priority.

This article featured in Australian Stainless magazine - Issue 44, Spring 2008.

ASSDA - Supporting You

ASSDA’s activities focus on networking, promotion, education, accreditation, standards development and problem-solving. View the Association's history of achievements and milestones in supporting the Australian stainless steel industry here.

160+

Member Organisations

100+

Publications

8,775+

Stainless Steel Specialist
Course enrolments

Check out our services

 

Stainless Steel Specialist Course

An online educational tool designed to improve your knowledge of stainless steel, its properties, performance and uses. Consisting of 17 challenging and rewarding modules, the course delivers a standard level of knowledge and qualification across the industry.

Learn more
 

ASSDA webinars

ASSDA's webinar program was introduced in late 2014, providing educational presentations on various stainless steel topics for Members, the specifying community and the stainless steel industry as a whole.

Learn more
 

Technical inquiries

ASSDA's Technical Support Service represents a significant asset to the local stainless steel industry, providing excellent and timely advice for the successful use of the product.

Learn more
 

ASSDA resources

ASSDA delivers a strong publications and training program with a range of titles available to participants in the stainless steel industry.

Learn more

Stainless Steel Industry Directory

As the go-to resource for the stainless steel industry in Australia, this directory is designed to showcase the capabilities of ASSDA Members and Accredited Fabricators while also serving as a platform to connect businesses with potential work opportunities.
Whether you’re a professional within the industry or a client seeking a specific stainless steel service, the Stainless Steel Industry Directory is here to facilitate connections and collaborations. Browse ASSDA’s Directory now to discover the businesses and services that can meet your stainless steel needs effectively and efficiently.

ASSDA Young Professionals Network

Empowering the next generation of stainless steel professionals and leaders.