Opportunity 1745 Tech ID# 16264
Wayne Larkin from Gray Design Space is looking for a supplier of seven hundred 316 hollow stainless steel balls, 150mm in diameter with walls about 1mm thick and a 35mm hole through a diameter. The surface polish must be smooth and, for reasons of corrosion resistance, must be electropolished. If you are interested, Wayne's number is 0409 668 846.

QUEENSLAND

Opportunity 1746 Tech ID# 16264
Hayden Morris from Inter-Marine Pty Ltd is looking for 70 flat bars in 253MA for a furnace. The dimensions are 80mm wide, 550mm long and preferably 15mm thick.  If you can supply ex stock or have plate that is suitable thickness for cutting, Hayden's number is 0416 921 954.