Gold Coast's Kirra Point: Looking Great Six Years On

Gold Coast's Kirra Point: Looking Great Six Years On

When the Gold Coast City Council was seeking a stable and visually stunning medium for use on their Kirra Point board walk project in 1999, they looked no further than stainless steel and after six years in service, it still looks great.

 

Council engineers chose stainless steel for the upright posts and moveable handrail system for safety, corrosion resistance and aesthetic reasons.

When designing the project, the board walk had to take into account a steep vertical drop to the beach below - an important safety issue met by using stainless steel handrailing.

The board walk project was undertaken in two stages, the first of which involved constructing a concrete walkway and handrails along the Kirra Point foreshore. The second stage saw the construction of a timber board walk out over the foreshore onto the beach.

ASSDA Accredited Fabricator, Stoddart (Tom Stoddart Pty Ltd) supplied 186 custom made upright posts and supplied and installed 326 metres of stainless steel tubular handrails. Both were made from 316 grade stainless steel with a number 4 finish.

The upright posts were passivated in nitric acid after manufacture to ensure a clean surface and promote corrosion resistance.

The knowledge that ASSDA requires for its Accreditation Scheme was used in the execution of the structure, ensuring the ongoing satisfaction of the Council with minimal maintenance.

This article featured in Australian Stainless magazine - Issue 35, Autumn 2006.

ASSDA - Supporting You

ASSDA’s activities focus on networking, promotion, education, accreditation, standards development and problem-solving. View the Association's history of achievements and milestones in supporting the Australian stainless steel industry here.

160+

Member Organisations

100+

Publications

8,775+

Stainless Steel Specialist
Course enrolments

Check out our services

 

Stainless Steel Specialist Course

An online educational tool designed to improve your knowledge of stainless steel, its properties, performance and uses. Consisting of 17 challenging and rewarding modules, the course delivers a standard level of knowledge and qualification across the industry.

Learn more
 

ASSDA webinars

ASSDA's webinar program was introduced in late 2014, providing educational presentations on various stainless steel topics for Members, the specifying community and the stainless steel industry as a whole.

Learn more
 

Technical inquiries

ASSDA's Technical Support Service represents a significant asset to the local stainless steel industry, providing excellent and timely advice for the successful use of the product.

Learn more
 

ASSDA resources

ASSDA delivers a strong publications and training program with a range of titles available to participants in the stainless steel industry.

Learn more

Stainless Steel Industry Directory

As the go-to resource for the stainless steel industry in Australia, this directory is designed to showcase the capabilities of ASSDA Members and Accredited Fabricators while also serving as a platform to connect businesses with potential work opportunities.
Whether you’re a professional within the industry or a client seeking a specific stainless steel service, the Stainless Steel Industry Directory is here to facilitate connections and collaborations. Browse ASSDA’s Directory now to discover the businesses and services that can meet your stainless steel needs effectively and efficiently.

ASSDA Young Professionals Network

Empowering the next generation of stainless steel professionals and leaders.