Stainless for the Long Haul


Posted 1 July 2003

The long-term cost effectiveness of stainless steel makes it a worthwhile proposition even though the initial outlay can be significant. The construction industry is realising that choosing a cheaper, but less durable material can be a false economy.

Eventually repairs need to be made and this can be at considerable expense. Further, there are likely to be logistical problems absent from the initial construction which add to the cost.

For example, when 101 Collins Street – a prestigious Melbourne high-rise office building – was completed twelve years ago, its two 80,000 litre fire water storage tanks were constructed out of bolted steel with a nylon-coated internal surface. Over time the coating had pitted and the steel was corroding, raising concerns about the future reliability of the system.

It was decided that replacement tanks should be fabricated from 4mm thick 316 stainless steel for long-term reliability.

Access was limited because the tanks had been placed in position with the attendant pumps and fire services system plumbing installed beneath them. In fact, a hatch in the floor above the tanks measuring just under a metre square was the only way in and out of the area.

ASSDA member, J Furphy & Sons of Shepparton, Victoria was the successful tenderer for the construction and installation of the new tanks.

The 7.4m long x 2.4m wide x 4.8m deep tanks were fabricated in individual panels, 4.8m x 900mm. With a hoist assembly above, the panels were lowered into position through the hatch and welded in situ. Other challenges to be overcome were creating adequate occupational health and safety conditions and providing welding power and services to the site.

The final step in the project was in situ hydrostatic testing for leaks which proved successful.

The owners of 101 Collins Street can now look forward to many years of worry-free service performance.

This article featured in Australian Stainless magazine - Issue 25, July 2003.

ASSDA - Supporting You

ASSDA’s activities focus on networking, promotion, education, accreditation, standards development and problem-solving. View the Association's history of achievements and milestones in supporting the Australian stainless steel industry here.

160+

Member Organisations

100+

Publications

8,775+

Stainless Steel Specialist
Course enrolments

Check out our services

 

Stainless Steel Specialist Course

An online educational tool designed to improve your knowledge of stainless steel, its properties, performance and uses. Consisting of 17 challenging and rewarding modules, the course delivers a standard level of knowledge and qualification across the industry.

Learn more
 

ASSDA webinars

ASSDA's webinar program was introduced in late 2014, providing educational presentations on various stainless steel topics for Members, the specifying community and the stainless steel industry as a whole.

Learn more
 

Technical inquiries

ASSDA's Technical Support Service represents a significant asset to the local stainless steel industry, providing excellent and timely advice for the successful use of the product.

Learn more
 

ASSDA resources

ASSDA delivers a strong publications and training program with a range of titles available to participants in the stainless steel industry.

Learn more

Stainless Steel Industry Directory

As the go-to resource for the stainless steel industry in Australia, this directory is designed to showcase the capabilities of ASSDA Members and Accredited Fabricators while also serving as a platform to connect businesses with potential work opportunities.
Whether you’re a professional within the industry or a client seeking a specific stainless steel service, the Stainless Steel Industry Directory is here to facilitate connections and collaborations. Browse ASSDA’s Directory now to discover the businesses and services that can meet your stainless steel needs effectively and efficiently.

ASSDA Young Professionals Network

Empowering the next generation of stainless steel professionals and leaders.