When used properly, stainless steel enjoys a strong and enduring reputation for visual appeal and structural integrity in a wide range of applications and environments.

But, like all materials, stainless steel may become stained or discoloured over time, impairing the overall look. This brown discolouration - tea staining - has been identified in coastal applications in Australia and overseas.

Factors affecting tea staining have been researched by ASSDA and the information gathered has been supported by experiences from around the world.

This article provides information on tea staining and what fabricators, specifiers and end users should do to help avoid

Stainless Steel Fabrication

Common Traps to Avoid


Posted 1 April 2006

Errors in stainless steel fabrication can be expensive and difficult to resolve. So a 'Get it right the first time' approach to stainless fabrication is necessary to gain the best result. Check the ASSDA website regularly for a local Stainless Steel Specialist.

ASSDA Accredited Fabricators - Ensuring the Best Result
ASSDA Accredited Fabricators
are companies and individuals that have a common understanding of successful technical practices for fabricating stainless steel.

To ensure the highest standard in quality, Accredited Fabricators belong to the ASSDA Accreditation Scheme, an ASSDA initiative that is intended

Training your stainless steel specialists with ASSDA

Training your stainless steel specialists with ASSDA

Transforming apprentices into stainless steel specialists can be a challenging but rewarding experience for employers seeking to improve quality, retain staff and increase profitability.

Underpinning theory and practical training in stainless steel represents only a small part of TAFE fabrication education in Australia. Understanding of standard industry terms such as pickling and passivation, crevice corrosion and knowledge of all the stainless steel grades by students even after completion is minimal.

In response to this problem, ASSDA developed the Stainless Steel Specialist Course, a 16 module training course that provides the industry with the underpinning knowledge required to meet the quality

Australian Stainless Products

Australian Stainless Products

Built on Reputation

Alistair Patterson has a flair for the food and beverage industry that borders on obsession. As the sole proprietor for ASSDA Accredited Fabricator, Australian Stainless Products, Patterson's reputation within the industry means when projects are on, he is onto it!

Australian Stainless Products are custom manufacturers of quality stainless steel food, beverage and pharmaceutical process products and equipment.

Established more than 20 years ago, Australian Stainless Products started out building basic dairy machinery, primarily small repairs and maintenance of equipment for a few of the local food processing equipment plants.

“Back then the business was basically building

Safe Disposal with Simcraft Stainless Steel Products

Safe Disposal with Simcraft Stainless Steel Products

As a general rule, the waste management method adopted for disposing of radioactive substances is critical. The main method of disposal is the dilution and dispersion of radioactive wastes using stainless steel equipment such as isotope flushing sinks

 

Last year, the University of Western Australia's School of Biomedical, Biomolecular and Chemical Sciences moved into the new $65M Molecular and Chemical Sciences building with state-of-the-art laboratories and equipment.

Generally, the materials used in biological sciences research work contain low radiotoxicity substances, however, full precautions are taken to ensure safe handling.

As part of the School of Biomedical, Biomolecular and Chemical

Manufacturing malt with stainless steel

Manufacturing malt with stainless steel

Australians really enjoy a good beer - at home barbeques, parties, music concerts, sporting events - in fact, everywhere!

World beer consumption is increasing by more than two per cent a year, a trend that is set to continue. There is an important relationship with beer consumption and demand for its main and critical ingredient - malt.

Malting is the partial germination and kilning of a grain, usually barley. Malt gives varying colour, flavour and body to beer depending on the style of malt being used.

Australia is a key player in the world market representing about 32 per cent

Gold Coast's Kirra Point: Looking Great Six Years On

Gold Coast's Kirra Point: Looking Great Six Years On

When the Gold Coast City Council was seeking a stable and visually stunning medium for use on their Kirra Point board walk project in 1999, they looked no further than stainless steel and after six years in service, it still looks great.

 

Council engineers chose stainless steel for the upright posts and moveable handrail system for safety, corrosion resistance and aesthetic reasons.

When designing the project, the board walk had to take into account a steep vertical drop to the beach below - an important safety issue met by using stainless steel handrailing.

The board walk project was undertaken

Food Specification Improves Fabrication Practices

Food Specification Improves Fabrication Practices

Hygiene and the 'cleanability' of equipment used in the production of food are paramount. The widespread use of stainless steel equipment in the food industry goes some way towards ensuring these criteria are met - but the assurances provided by stainless steel are only as good as the fabrication quality of the equipment.

Following a presentation at ASSDA’s annual conference in 2003 on the quality of food fabrications, particularly in the dairy industry, it became apparent that fabrication specifications, if they existed, were often inadequate and inconsistent.

As a result, ASSDA launched a co-operative venture, working closely with many fabricators

No. 4: The workhorse finish

No. 4: The workhorse finish

No. 4 finish stainless steel is the workhorse of the light fabrication industry. The easiest of the finishes to maintain, No 4 finish is used for work surfaces, handrails and where appearance is important.

A 'No. 4' surface is produced by cutting the surface with abrasive belts to remove a very small amount of metal without affecting its thickness.

For architects and designers, No. 4 finish gives low gloss and best apparent flatness of panels.  For fabricators, the No 4 finish is directional, allowing easy matching of surfaces and refinishing of welds. For end users, the surface can be repaired

Stainless steel 'Travellers' mark journey of migration

Stainless steel 'Travellers' mark journey of migration
Telling the tale of migration to Victoria is 'The Travellers', a series of giant stainless steel sculptures sliding quietly across the Sandridge Rail Bridge on Melbourne's Yarra River.

Stainless Steel 'Travellers' Mark Journey of MigrationUnveiled just three days from the start of the Melbourne 2006 Commonwealth Games, the 10 sculptures are a tribute to multiculturalism.

Each of 'The Travellers' figures represents a period from our Indigenous and immigrant histories (as defined by historian Dr James Jupp) and were designed by Lebanese Artist, Nadim Karam of Atelier Hapsitus.

'Gayip - The Aboriginal Period', the first sculpture, is stationed permanently on the river bank to depict the Indigenous

Quality Fabrication Keeps the Meat Rolling

Quality Fabrication Keeps the Meat Rolling

Loss in production due to installation of new equipment is always undesirable, which is why an upgrade on the scale of Australia Meat Holdings’ recent boning room expansion at Aubigny (west of Toowoomba, Qld) was even more remarkable.

 

The project, managed by Wiley & Co, more than doubled the size of AMH’s existing boning room, improved work place ergonomics and provided for future growth – all without interruption to production.

The expansion incorporated more than $4 million worth or 100 tonnes of stainless steel, around half of which was fabricated by ASSDA Accredited Fabricator G & B Stainless from

Stainless rebar enhances technology performance

Stainless rebar enhances technology performance

Stainless steel's non-magnetic properties were an important factor in the design, building and construction of the University of New South Wales' (UNSW) new Analytical Centre.

The facility has been designed to enhance the performance of high-tech analytical equipment such as the UNSW's nuclear magnetic resonance instruments (NMRs).

The centre is one of six components in the North Mall Development Zone (NMDZ) project, located within the Kensington Campus of the University of New South Wales (UNSW).

According to Mr Ed Smith of McLachlan Lister, the Project Directors of the NMDZ, building will accommodate both staff and equipment from the University's

445M2: A New Generation Stainless Steel (Part 1)

445M2: A New Generation Stainless Steel (Part 1)

This article is the first in a series showcasing the uses of 445M2 stainless steel. Read Part 2. Read Part 3.

Australians' love of the water has always provided challenges to the construction industry, particularly when it comes to choosing materials that can be used in aggressive environments such as near the coast or swimming pools.

Stainless steel grades 316 and 304 have long been the obvious solution in these applications, but the key factors of formability, cost and corrosion resistance are now shining the spotlight on an alternative grade.

445M2 stainless steel has been used in Australia for a

Design Software Vs. Back to Basics

Design Software Vs. Back to Basics

New technology to assist with accurate design is always welcome, but it is important that users proceed with caution when using international design tools.

There is no doubt that designing with stainless steel offers endless opportunities for architects and engineers to be both creative and functional. At the same time, it is critical that the design is right for the application.

Thanks to the internationally-recognised research of an Australian expert, as well as some design software now available free online, getting the design right for stainless steel structures has never been easier. However, as outlined below, it is more important

Big Fish Swimming in a Small Pond

Big Fish Swimming in a Small Pond

Northern Territorians know their barramundi, which is why ASSDA Accredited Fabricator Northern Stainless had to get it absolutely right when they reeled in the contract to design and fabricate this 1030mm specimen.

The silver fish has a mythical reputation in the NT, not least because of its shimmering, silver appearance.

Northern Stainless operations manager Darren Colbert said they had no hesitation in saying they could get the job done to their client's satisfaction, because of their ability to create the barra's mesmerising shimmer in stainless steel.

We knew stainless was the right material for the job because we needed the

Mrs Crocket's Stainless Kitchen

Mrs Crocket's Stainless Kitchen

Twelve months after the design and installation of a unique cabbage processing system in Melbourne, the importance of quality stainless steel fabrication has never been clearer.

 

ASSDA Accredited fabricator Bridgeman Stainless Solutions (Brendale, Queensland) was commissioned to design the unique facility at Mrs Crocket's Kitchens, which was completed in October 2005.

The $500,000 project incorporated various plate, sheet, pipe and RHS stainless in grades 304 and 316, and was specified to reduce the risk of contamination in the handling processes for all coleslaws, pastas and food products.

Bridgeman's Managing Director Len Webb said there was previously no system available

445M2: A New Generation Stainless Steel (Part 2)

445M2: A New Generation Stainless Steel (Part 2)

This article is the second in a series showcasing the uses of 445M2 stainless steel. Read Part 1. Read Part 3.

The use of stainless steel plant and equipment in the food industry continues to prove its worth as an increasing number of processors adopt its use in line with the dedication and obligation to food quality and safety.

Whilst stainless steel grades 316 and 304 offer an environment of easy maintenance and cleaning, 445M2 stainless steel goes one step further.

445M2 panels have been supplied to Bertocchi Smallgoods by ASSDA Major Sponsor Austral Wright Metals, following a four-month trial

Smooth and Corrosion Resistant Surfaces from the Mill

Smooth and Corrosion Resistant Surfaces from the Mill

This article is the second in a series on common finishes. The first (Winter edition 2006) dealt with the abraded 'No. 4' (2K, 2J) finish. This article looks at 2D, 2B and BA: smooth and corrosion resistant surfaces produced at the steel mill. Subsequent articles in this series will cover mirror polished (No. 8 or 2P) and profiled and hot rolled (No. 1) finishes.

What are Cold Rolled Finishes?
Cold rolled finishes apply to flat products such as sheet or coil, with thickness less than about 5mm and usually less than 3mm.  They are firstly hot rolled into a strip

Stainless Steel Launches its Artistic Merit

Stainless Steel Launches its Artistic Merit

Internationally renowned, Yackandandah based sculptor Benjamin Gilbert was commissioned to create a series of sculptures for Melbourne’s Commonwealth Games.  Extending six metres in the air, the exhibits laid testament to three different stages of a pole–volter whilst displaying the versatility and artistic merit of stainless steel.

Benjamin used grade 304 stainless steel, supplied by ASSDA major sponsor Atlas Specialty Metals in Wadanga.  He has worked with stainless steel for 10 years and believes it is cost effective and cheaper to use than other materials. Also, the added ability of using off cuts in his work suited Benjamin’s ‘green’ focus.

“As

A Great Aussie Tradition Makes its Way

A Great Aussie Tradition Makes its Way

For those who love to indulge in a life of sun, surf and sand the idea of placing a barbeque in such rust-promising environments is not often an option as their longevity is compromised.

But Gold Coast company Southern Stainless has bridged the gap between a nautical lifestyle and the great Aussie tradition by manufacturing barbeques in stainless steel.

ASSDA member Southern Stainless typically specialises in the manufacture of stainless steel products including wine storage and fermentation tanks and marine fitouts, but supplying stainless steel barbeques, boat mounting systems and accessories to the general public, wholesalers, retailers and building industry

ASSDA - Supporting You

ASSDA’s activities focus on networking, promotion, education, accreditation, standards development and problem-solving. View the Association's history of achievements and milestones in supporting the Australian stainless steel industry here.

160+

Member Organisations

100+

Publications

8,775+

Stainless Steel Specialist
Course enrolments

Check out our services

 

Stainless Steel Specialist Course

An online educational tool designed to improve your knowledge of stainless steel, its properties, performance and uses. Consisting of 17 challenging and rewarding modules, the course delivers a standard level of knowledge and qualification across the industry.

Learn more
 

ASSDA webinars

ASSDA's webinar program was introduced in late 2014, providing educational presentations on various stainless steel topics for Members, the specifying community and the stainless steel industry as a whole.

Learn more
 

Technical inquiries

ASSDA's Technical Support Service represents a significant asset to the local stainless steel industry, providing excellent and timely advice for the successful use of the product.

Learn more
 

ASSDA resources

ASSDA delivers a strong publications and training program with a range of titles available to participants in the stainless steel industry.

Learn more

Stainless Steel Industry Directory

As the go-to resource for the stainless steel industry in Australia, this directory is designed to showcase the capabilities of ASSDA Members and Accredited Fabricators while also serving as a platform to connect businesses with potential work opportunities.
Whether you’re a professional within the industry or a client seeking a specific stainless steel service, the Stainless Steel Industry Directory is here to facilitate connections and collaborations. Browse ASSDA’s Directory now to discover the businesses and services that can meet your stainless steel needs effectively and efficiently.

ASSDA Young Professionals Network

Empowering the next generation of stainless steel professionals and leaders.